When a line produces leakers, wrinkles or burnt-looking seals, the instinct is to adjust the machine. More often the real fix is in the film specification. Film and machine are one system: the sealant layer, thickness, stiffness and friction all have to match the forming path, jaw temperature and dwell time.

The three layers of a packaging film

Most flexible packaging films are laminates built from three functional layers, even when the reel looks like a single sheet:

  • Outer / print layer, provides stiffness, gloss, printability and abrasion resistance. Usually OPP, PET or paper.
  • Barrier layer, controls oxygen, moisture, light and aroma transmission. May be EVOH, metallised PET (VMPET), aluminium foil, PVDC coating or a high-barrier nylon.
  • Inner / sealant layer, melts to form the seal. Usually PE (LDPE/LLDPE), CPP or an ionomer. This layer determines the sealing temperature, seal strength and hot-tack.

A simple biscuit flow wrap may be just OPP/CPP, two layers, low cost, fast sealing. A coffee pouch may be PET/VMPET/PE or PET/AL/PE, three or four layers, high barrier, narrower sealing window and higher cost. The more layers you add, the more carefully the machine has to be set up.

Common materials and what they do

MaterialRoleNotes
OPP / BOPPOuter print layerCheap, glossy, good stiffness; poor barrier on its own
CPPSealant / inner layerHigher heat resistance than PE; common on flow wrap
PETOuter layer, strengthHeat stable, good print surface, adds stiffness
PE (LDPE / LLDPE)Sealant / inner layerWide sealing window, good hot-tack; common on VFFS
EVOHOxygen barrierSensitive to moisture; usually buried between layers
VMPET / aluminium foilLight & oxygen barrierExcellent barrier; foil adds stiffness and crease risk
Nylon (PA)Puncture resistanceUseful for sharp or heavy products; absorbs moisture

Match the film to the machine

Different forming paths put different demands on the reel:

  • Flow wrap films must fold cleanly around a forming box and slide over metal surfaces with low, consistent friction. OPP/CPP and OPP/PE are typical. Because the seal is made under the product with a fin seal, the sealant layer must seal to itself at high line speed.
  • VFFS films must form into a tube over a collar, resist stretch under the film pull belts, and seal through the vertical and horizontal jaws. PE sealants are common because of their wide sealing window and good hot-tack, important when a heavy product drops into a bag whose bottom seal is still warm.
  • Premade pouches are already converted and printed, so you specify the laminate structure with the pouch supplier rather than buying a reel. The critical check is that the inner sealant works with the rotary machine's jaw temperature and dwell time. See the pouch format guide for how format interacts with sealing.

Also confirm the reel specifications: core inner diameter, maximum outer diameter, roll weight, splice type and film width tolerance. A reel that is too heavy for the unwind brake or too wide for the forming set will cause tracking faults that look like machine faults.

Sealing window: the number that matters most

Ask your film supplier for the seal-initiation temperature (SIT), the recommended jaw temperature range, and the hot-tack curve. The sealing window is the range of temperature, pressure and dwell time in which you get a strong, clean seal without burning or distorting the film.

A wide window (typical of PE sealants) is forgiving: small changes in line speed or ambient temperature still produce good seals. A narrow window (some high-barrier laminates, thin CPP structures or metallised films) means a 10 °C drift or a 10% speed increase can move you out of spec. On high-speed lines, a narrow window is a permanent source of intermittent leakers.

Practical rule: set jaw temperature to achieve a seal at the lowest temperature that still passes a peel/drop test, then keep the film lot, ambient conditions and line speed stable. Chasing seal faults by simply turning up the heat usually shortens sealing element life and distorts the film.

Other film properties to put on the specification sheet: thickness (µm) and tolerance, coefficient of friction on both sides, tensile stiffness, curl / bow, corona treatment level for printing, registration mark contrast and spacing, and maximum recommended line speed. Ask for a certificate of analysis per lot so a bad reel can be identified quickly.

Barrier and shelf life

Start from the product's failure mode, then specify OTR (oxygen transmission rate) and WVTR (water vapour transmission rate) targets with your film supplier.

  • Fats, nuts, coffee, snacks, oxygen and light drive rancidity; consider VMPET, foil or EVOH plus a light-blocking layer.
  • Powders, crackers, dried foods, moisture drives caking and loss of crispness; WVTR matters most.
  • Aroma-sensitive products, specify aroma barrier, not just oxygen barrier; foil and EVOH perform differently here.
  • Fresh produce, sometimes you need controlled permeability (anti-fog, micro-perforation) rather than maximum barrier.

If you plan modified atmosphere packaging (nitrogen flushing), verify the achievable residual oxygen with a test batch. Barrier film, flushing nozzle position and seal integrity all have to work together. Machine-side considerations are covered in our flow wrap vs VFFS comparison.

Cost per pack, not cost per kilo

Film is usually quoted per kilogram, but what matters is cost per 1,000 saleable packs. Calculate:

  1. Pack dimensions → film area per pack (include the fin seal overlap and cross-seal waste).
  2. Film yield (m²/kg) from grammage → kg per 1,000 packs.
  3. Multiply by reel price, then add start-up, splice and changeover waste (often 2–5%).
  4. Add the cost of rejects caused by a narrow sealing window: a cheaper film that produces 2% leakers is not cheaper.

Thinner film reduces material cost but can reduce stiffness and barrier, forcing a slower line speed. Always compare the full line output, not the reel price alone.

Troubleshooting quick reference

SymptomLikely film-side cause
Weak or peeling sealsJaw temperature below SIT, wrong sealant layer, contaminated seal area
Burnt / distorted filmTemperature too high for dwell time, film too thin, jaw pressure uneven
Wrinkles on the packHigh or uneven COF, curl/bow in the reel, film tension too high
Print drifting off-centreWeak registration mark contrast, incorrect mark spacing, film slip
Bag forming badly on VFFSFilm too stiff, thickness tolerance wide, collar size mismatched to lay-flat width

Keep a log of film lot numbers against these symptoms: it makes supplier conversations much shorter. For routine checks that keep the sealing system in condition, see our maintenance checklist.

Send us your film spec. If you already have a reel datasheet, our engineers can confirm compatibility with the machine and suggest a sealing window before you place an order. Ask an engineer →

Film choice by product category

Film data sheets describe barrier and seal strength. They do not tell you what happens when the product is oily, frozen or dusty. This table covers the five categories we quote most often.

ProductTypical structureWhyWhat goes wrong
Coffee, whole beanPET/AL/PE or PET/VMPET/PEOxygen and aroma barrierBag inflates if CO2 has nowhere to go
Frozen foodPET/PE, low seal initiationSeals at a low jaw temperatureCondensation sits in the jaw and blocks the seal
Snacks and chipsOPP/CPP or metallised OPPCrisp feel plus moisture barrierCrumbs in the seal area
Sauce and liquidsPET/AL/PE or PET/PEPuncture and channel resistanceFill temperature outside the seal window
Detergent powderStiffer PET/PEHolds a 1 kg fill without bulgingDust in the seal and on the jaw

Is a thicker film always stronger?

No. Puncture resistance comes from the structure, not the calliper. A 90 micrometre PET/PE can outperform a 120 micrometre mono film, and it usually seals at a lower temperature, which matters on high-speed lines.

What is the cheapest film that still works?

For dry products with a short shelf life, a two-layer OPP/CPP. For anything containing oil or aroma, or needing six months of shelf life, a metallised or foil structure pays for itself in fewer returns and fewer complaints.

If the film is right and the seal still fails, the machine settings are next. See ten maintenance habits for the jaw and temperature checks, and flow wrap vs VFFS for how each machine handles film.

Frequently asked questions

SIT is the lowest temperature at which the sealant layer forms a seal of acceptable strength under a given pressure and dwell time. It defines the bottom of your sealing window and should be supplied by the film converter.
Sometimes, but not automatically. The forming path, friction, stiffness and sealing geometry differ. Confirm with a trial on each machine rather than assuming a reel is interchangeable.
Dwell time falls as line speed rises, so the jaw temperature must sit higher in the sealing window. If the window is narrow, you run out of margin, a common reason for intermittent leakers that disappear at slow speed.
State the product failure mode and target OTR/WVTR values, then ask the converter for a laminate proposal and a sample run. Verify with shelf-life testing and a seal-strength test on the actual machine.

Next step: tell us about your product or browse all packaging machines.